| Iron
Segment Fracture Surface |
Processing conditions:
| Bond |
100% iron |
| Sintering Temperature |
1100 °C |
| Time |
10 min |
| Atmosphere |
Argon |
| Uncoated
MBS Diamond
|
Coated MBS Si2 Diamond
|
 |
 |
| Severe
reaction causing no chemical attachment
to bond |
No
reaction – MBS Si2 coated diamond
shows good attachment to bond |
|
| Crystals
Recovered from Iron Segment |
| Uncoated
MBS Diamond
|
Coated
MBS Si2 Diamond |
 |
 |
| Severe
reaction – complete loss of crystal
edges, corners and faces |
MBS
Si2 diamond resists chemical attack
even in 100% iron bond |
|
|
|
| MBS Si2
Coated Diamond processed at 970°C
|
MBS Si2
Coated Diamond processed at 1050°C |
 |
 |
| Examples
of crystal protection in high iron bonds for
dry concrete cutting. |
For general bond recommendations for superior
performance of MBS coated diamonds,
click here
Availability chart in US Mesh and FEPA sizes,
click here
Diamond Innovations has a patent
pending on the use of Si2 coated diamonds in metal
segments. Under the terms and conditions of your
Diamond Innovations Si2 product purchase, customers
receive an implied license for its use. |